ASTM-A388 2011
$40.63
A388/A388M-11 Standard Practice for Ultrasonic Examination of Steel Forgings
Published By | Publication Date | Number of Pages |
ASTM | 2011 | 9 |
1.1 This practice covers the examination procedures for the contact, pulse-echo ultrasonic examination of steel forgings by the straight and angle-beam techniques. The straight beam techniques include utilization of the DGS (Distance Gain-Size) method. See Appendix X3.
1.2 This practice is to be used whenever the inquiry, contract, order, or specification states that forgings are to be subject to ultrasonic examination in accordance with Practice A388/A388M.
1.3 Supplementary requirements of an optional nature are provided for use at the option of the purchaser. The supplementary requirements shall apply only when specified individually by the purchaser in the purchase order or contract.
1.4 The values stated in either SI units or inch-pound units are to be regarded separately as standard. The values stated in each system may not be exact equivalents; therefore, each system shall be used independently of the other. Combining values from the two systems may result in non-conformance with the standard.
1.5 This specification and the applicable material specifications are expressed in both inch-pound units and SI units. However, unless the order specifies the applicable M specification designation [SI units], the material shall be furnished to inch-pound units.
1.6 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.
PDF Catalog
PDF Pages | PDF Title |
---|---|
1 | Scope Referenced Documents Terminology Significance and Use |
2 | Ordering Information Apparatus Personnel Requirements Preparation of Forging for Ultrasonic Examination Procedure |
4 | Recording Report Quality Levels |
5 | Keywords X1. TYPICAL TUNING LEVEL COMPENSATION FOR THE EFFECTS OF FORGING CURVATURE X1.1 X1.2 |
6 | X2. INDICATION AMPLITUDE COMPENSATION FOR TEST DISTANCE VARIATIONS X2.1 X2.2 FIG. X1.1 FIG. X2.1 |
7 | X3. BACKGROUND INFORMATION ON THE DGS METHODS X3.1 X4. COMPENSATION FOR CENTER HOLE ATTENUATION ON CYLINDRICAL BORED OR HOLLOW FORGINGS UTILIZING THE DGS METHOD X4.1 FIG. X3.1 |
8 | FIG. X4.1 |