A744/A744M-10e1 Standard Specification for Castings, Iron-Chromium-Nickel, Corrosion Resistant, for Severe Service
Published By | Publication Date | Number of Pages |
ASTM | 2010 | 6 |
1.1 This specification covers iron-chromium-nickel alloy, stainless steel castings intended for particularly severe corrosive applications.
1.2 This specification requires postweld heat-treatment of all weld repairs affecting surfaces intended to be wetted by the corrosive medium. For applications for which postweld heat-treatment is not considered mandatory for retention of acceptable corrosion resistance, refer to Specification A743/A743M .
Note 1For general corrosion-resistant alloy castings, reference should be made to Specification A743/A743M . For general heat-resistant alloy castings, reference should be made to Specification A297/A297M . For nickel-base alloy castings, refer to Specification A494/A494M .
1.3 The values stated in either SI units or inch-pound units are to be regarded separately as standard. The values stated in each system may not be exact equivalents; therefore, each system shall be used independently of the other. Combining values from the two systems may result in non-conformance with the standard.
1.3.1 Within the text, the SI units are shown in brackets.
1.3.2 Inch-pound units are applicable for material ordered to Specification A744 and SI units for material ordered to Specification A744M.
PDF Catalog
PDF Pages | PDF Title |
---|---|
1 | Scope Referenced Documents Terminology General Conditions for Delivery |
2 | Ordering Information Process Heat Treatment Chemical Requirements Workmanship, Finish, and Appearance Repair by Welding TABLE 1 |
3 | TABLE 2 |
4 | Rejection and Rehearing Product Marking Keywords |
5 | X1. RECOMMENDED FILLER METALS FOR CAST STAINLESS STEELS X1.1 TABLE S22.1 TABLE X1.1 |